Scout Trooper – Armor – Back – Smoothing, Completed

Sanding, Putty, More Sanding, And Primer…

Make it smooth…

Wet sanding with 220 grit sandpaper.

Glazing putty applied to the remaining low spots.

Wet sanded with 220 grit sandpaper.

Fourth coat of primer. This looks to be ready for paint.